Abstract

ABSTRACT
Lightweight brick waste (LBR) from leftover materials after installation in
construction projects generally accumulates as environmental waste, is difficult to
decompose, and has low economic value. This study aims to analyze the effect of
substituting fine aggregate with LBR at levels of 0%, 12%, 18%, and 24% with a
constant 8% addition of silica fume across all variations on the characteristics of
concrete. The method used was a laboratory experiment with 15×30 cm cylindrical
test specimens in accordance with SNI 03-7656-2012. The tested parameters
included slump, unit weight of hardened concrete, compressive strength, and split
tensile strength at 7, 14, and 28 days; these were analyzed using simple linear
regression via SPSS and compared in terms of production costs based on the 2026
Bekasi City Fine Aggregate Price List. The research results show that the slump
value increased from 12 cm in the control concrete to 13 cm with 12% LBR
substitution, then decreased to 12 cm with 18% LBR and 10 cm with 24% LBR,
with all variations meeting the specified slump requirements. The unit weight of
hardened concrete decreased consistently from 2,307 kg/m³ in the control concrete
to 2,181 kg/m³ at 24% LBR, but it still falls within the range of normal concrete.
The compressive strength of the concrete at 28 days decreased from 25.21 MPa in
the control concrete to 19.90 MPa, 17.82 MPa, and 14.14 MPa, respectively, for
LBR 12%, 18%, and 24%, with a coefficient of determination R² = 0.992
(significance 0.004). Splitting tensile strength decreased from 3.17 MPa to 2.49
MPa, with R² = 0.974 (significance 0.013). The 12% LBR mixture with 8% silica
fume proved to be the most optimal composition, exhibiting the smallest decrease
in compressive strength and yielding a production cost savings of 1.493% compared
to the control concrete
Keywords: Lightweight brick waste, Concrete, Concrete characteristics

Tipe Dokumen: Skripsi
Tipe: Skripsi
Jurusan: Program Studi Teknik Sipil
Depositing User: Dept Perpustakaan Jakarta Global University
Date Deposited: 15 Oct 2026 04:34
Last Modified: 15 Oct 2026 04:34
URI: https://digilib.jgu.ac.id/id/eprint/712

Actions (login required)

View Item
View Item